Friday, October 21, 2022

Re: [MW:33612] Missing Material Certificate of Existing Line

Dear Hasanov,

The PMI accuracy rate is high and releable.If you want to counter check of PMI, Kindly get a sample of piece from the existing line,take it to approved laboratory for the chemical analysis.

Thanks,

Kind Regards,

G.Gughan

On Fri, 21 Oct 2022 at 11:27, Ilkin Hasanov <ilkinhasanov.91@gmail.com> wrote:
Dear Faisal Sattar
Thanks for your prompt reply.

What is accuracy of this method ( PMI (OES))



On Fri, 21 Oct 2022 at 12:12 Faisal Sattar <faisalsattar315@gmail.com> wrote:
You may go through the spectroscopic test for the existing pipeline. It may give you material compositions. Based on that composition you may find the material grade and yield.

On Fri, 21 Oct 2022, 11:36 am ilkinhasanov, <ilkinhasanov.91@gmail.com> wrote:
Dear All,

We have to weld our new fabricated pipeline to existing live line. (welding code is 1104).

Unfortunately,  we do not have a certificates of existing line. and it is not possible to perform shutdown to take a test coupons and perform chemical analysis and mechanical tests to identify grade of materials.

All knows that, existing line's material is Carbon steel but exact Yield and tensile Strength and Chemical prosperities are unknown. (our new fabricated pipeline is also Carbon steel.

Could you please advise me what can we do in this condition?



Regards,
Ilkin HASANOV

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d15ccca5-11f3-4b41-9fd5-7e88e8715ae8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/wfO_RQUuwMw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE%2B-gCazdMMi_a%3DnUeT-eFB88oVeNGNu3zr2jCeQSTe3QMKqmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDa0%2BhXRvRDT83dOCHAE-H-DsGOE51GqTwYFSdk1kUPkxw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB0bcTOy3KsDx_-Vyp--sJhoGRtSUiERUgqUKup4_U4BCSyWkA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...