Tuesday, October 11, 2022

[MW:33584] P91- WPS & PQR

Team,

We are planning to go for a new PQR in P91 Materials (P. NO-15E).

SA 335 Gr. P91

Please let me know any guidance on P91 qualification and requirements and sample WPS and PQR
--
Thanks and Regards,
E. Anand,
QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChzbp9mT2D4-ihKe6XWBcQMOxjHeU3%3DiRjLRYMQiKzBOew%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...