Pradip, 
The spec seems to be outdated. There're scopes for improvement. You may refer latest API RP 582 for guidance, as well as the other industry standards & consumable manufacturer's guidebooks. 
Hope this will help. 

Thanks. 
P.Goswami, P.Eng,IWE



Sent from my Bell Samsung device over Canada's largest network.


-------- Original message --------
From: pradip kumar Sil <pradipsil@gmail.com>
Date: 2022-10-24 11:51 p.m. (GMT-05:00)
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:33619] Limitation of FCAW process

Dear all,

Our contract document is restricted for FCAW process upto 25 mm thickness and design temperature not less than minus 10 degree centrigrad for all pipe welding.

Any specific reason for the  limitation of particular process.

Thanks in advance.
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DKz1LWV0ofaEnFpSnWDXoaAo_utePdx_MKfbg%2B7CzmEQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...