Re: [MW:33568] RECERTIFICATION OF MATERIAL TEST CERTIFIACTE AS PER ASME

Since MTC is being ASME material with 2019 edition, you can use it directly. Only you have to endorse that Mtc reviewed as per 2021, Refer your ASME manual and read Material control section.

Thanks 

On Fri, Oct 7, 2022, 1:01 PM Saurabh Joshi <saurabh.joz30@gmail.com> wrote:
Dear All ,

     We have to manufacture a Heat ex-changer Code of construction ASME 2021(Code stamp required for the Equipment) . Raw material for plates & pipes are manufactured As per ASME 2019 . MTCs are available as per ASME 2019 and Original marking is still available on materials how can i re-certify the material and use it for the equipment which has the code of construction ASME 2021 .


Regards
Saurabh Joshi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3f6c2884-c436-4ef3-9905-5e2c51713a72n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPHaPBJM_ixnE8a04bWgAM2F8ghHCYw1S0fc22OT%3DtzKXrVf%3Dw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...