Skip to main content

Re: [MW:32794] Impact test PQR thickness criteria as per QW 403.6

only for base metal

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Jan 27, 2022 at 11:33 AM rahul ugale <rahulugale23@gmail.com> wrote:

Dear all ,


Please comment.



QW-403.6 The minimum base metal thickness qualified

For a WPS where impact test is applicable. As per QW-403.6 The minimum base metal thickness qualified is the thickness of the test coupon T or 16mm whichever less and if T less than 6mm, then 1/2T.

In the scenario, while filling the Weld Deposit range qualification in WPS, How we can enter the data. We can apply for the combination of both processes weld deposit thickness. But how to enter for individual process qualified range.


Ex: 1 ) Base Material Thickness – 53 mm  GTAW (13mm),SMAW(20 mm) & SAW (20 mm) , So PQR Range is 16 mm – 200 mm, what will be the individual ranges for each process considering QW 403.6

Ex: 2 ) Base Material Thickness – 20 mm GTAW (8 mm) & SMAW (12 mm) So PQR Range is 16 mm – 40 mm, what will be the individual ranges for each process considering QW 403.6


Regard,

Rahul

On Tue, Jan 25, 2022, 11:55 AM Yunsok Bang <stevebang87@gmail.com> wrote:
Hello. I am one of the welding quality managers who cooperate with representative semiconductor companies. Our customer has their own acceptance criterion that refer some international code such as ASME Section IX, BPE, 31.3, SEMI F81 etc. Recently, one of the related codes was questioned. It refers about the "Light Straw Color" in SEMI F81 regarding to the acceptance criteria of automatic welding surface color. We are using M200 automatic welding machine. There is no included any picture and details of it. Therefore, I wasn't able to find any exact standard of it. How could I verify that criteria. It's surface standard. It's not about the back bead which has certain criterion like AWS D18.2 or ASME BPE.

I would like to get some advices related to this from your various experiences.

Thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACrdFNT7j1Ms005dt7WZNw-QNvcJFgohHpHkyhkk0NWvxNVVeA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALu9g8N8o%3DGxcuMv21P3YvS2tCRq7an%2BmSfcdK4Zg6oNEe%2BD3A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNcbPfLBzJnFEwrdiubZ67UeaMJZYVQtqhS0X4mXxRCcg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...