[MW:32752] RE: 32751] Selection of Pigs For 30" Gas Pipeline

Pigging is a very special process. You need to talk to the companies specialized in this discipline. TDW specializes in this area. You may contact them, for specific services in Bangladesh, if they provide so. I know they've a big presence in India. This presentation discusses with some interesting issues, related to pigging .

Hope it will help you.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Engr. Asif Chowdhury
Sent: January 16, 2022 8:55 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:32751] Selection of Pigs For 30" Gas Pipeline

 

Dear Experts,

 

Hope everyone is doing great.

 

In a cross-country gas pipeline project over a bridge deck we have almost completed ou welding activities and right now we are facing problem in selection of Pigs for that pipeline. For your information, the pipeline is about approximately 6 Km in length consisting of 14 nos U-loop and 06 Nos W-loop and 01 nos inlet and 01 nos outlet loops. Outer Dia of Pipeline is about 762 mm with a wall thickness of 25.4 mm.

 

The elbows in the loops are 1.5D 90 Degree LR BW elbows.

 

The entire pipeline has some pipe miter joints included but the angle of miter falls between the range of 2.5 Degree to  5 Degree.

 

 The normal pigs we use for our cross-country pipeline having 3D & 5D Bends are not suitable here.

 

As I have limited knowledge on pigging, hope some expert comment can help me to select the appropriate pig and finalize procurement for my project in Bangladesh.

 

 

With best regards,

Asif

PM

PMB-NGP Project

WhatsApp: +8801925-884133

The Royal Utilisation Services (Pvt.) Ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c8df72f-7f96-4f82-8b8f-42521c4bc20bn%40googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...