Re: [MW:32736] Requalification of consumable after shelf life

Normally we do not use welding consumables beyond the Shelf life as recommended by welding consumable manufacturer. I have physically seen Flux coating peeling off from the electrode. It is better to contact the welding consumable manufacturer and if they recommend better to do consumable testing as per ASME Sec.IIC at the manufacturer's premises.

Thanks & Regards

J.Gerald Jayakumar




On Friday, 7 January, 2022, 12:08:41 pm GMT+4, Syed Gohar Abbas Zaidi <gohar.qaqc@gmail.com> wrote:


Dear,

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

On Thu, Jan 6, 2022 at 12:10 PM SN <suryawanshinileshj@gmail.com> wrote:
Dear all,

Can we requalify  welding consumables (electrode and wires) once the shelf life is over.

As ASME code gives any guideline to requalify  the welding consumables.

Kindly provide your expert opinion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


--



Regard's:

Syed Gohar Abbas Zaidi
Cell No.: 0092-324-1407544

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGOPWRvqgUthDZ8UL7vfdNbVTsaZ9H1RrA2%2BukY7xYndxEDjZQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .