Re: [MW:32756] impact test difference in WPS & MTC

NO
the specific batch test not yet as per ASME Sec-II part C.
only WPS qualified on -52°C 

Thanks & Regards

Sangramkeshari Routaray


MOB NO. +91-8249921885



On Monday, 17 January, 2022, 03:22:55 pm IST, Vishwas Keskar <vvkeskar123@gmail.com> wrote:


Is this specific batch is tested and certified as per ASME.SEC II  Part C for Impact testing at - 52 Deg C ?

On Mon, 17 Jan 2022, 15:02 'sangram routray' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear Experts,
we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact value @ -40°C.

Job's Impact requirement is -52°C.

shall I use the same specific batch Filler wire for the job?? (Y/N)
or required batch test qualification (all weld test )
Answer with code's justification.

 welding code ASME Sec-IX

code of construction ASME B31.3

Thanks & Regards

Sangramkeshari Routaray


MOB NO. +91-8249921885

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/215105493.712317.1642408446087%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3N5Tc9BbcRpC8Vw_gmBeq%2BGRCDQjWxzZGBmfB6nNL9sVg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .