Re: [MW:31519] Difference between ISO level III and ASNT level III personnel

Check T-120 until the end, in ASME BPVC Section V - Article 1

Στις Σάβ, 26 Σεπ 2020 στις 9:00 π.μ., ο/η Manish Kumar <mkmkr431@gmail.com> έγραψε:

Dear Sir,
I would like to know what is the difference between ISO level III and ASNT Level III personal.As per client  recommendation ASNT level III personnel is authorised for interpretation of PAUT.In this case,Is ISO level III authorised for interpretation of PAUT ?

Please advise us.
--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5qh9u17t6JCgpzBwXxr5obVRcx-sroz7k-yhg3FFT25g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AaPsiq23ZeVNEobVX-zgSpg%3DRe63dESoRoN-Gkw9OXgg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...