Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

No comments:

[MW:35693] egwuanimkwujacobisrael@gmail.com

Dear all, No. MPI can only detect defect that is 1 to 2 mm dept. Therefore the paint must have mask the defect. Thanks. Egwuanimkw...