Re: [MW:31490] Minimum thickness for PAUT

You are right , 
  B31 Case 181‐2  "Use of Alternative Ultrasonic Examination Acceptance Criteria in ASME B31.3 "
TABLE 1   includes acceptance criteria for surface flaws above 25mm .  As per my knowledge , there is no change 

On Fri, 18 Sep 2020 at 18:05, Manish Kumar <mkmkr431@gmail.com> wrote:
Dear Sir,
As per code B31.3 case 181, Minimum thickness for PAUT has been written 25mm.Kindly,give the advise for minimum thickness for PAUT as per latest revision of said code.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5Gcu8cUpp-so%2Br8drBbmwMWqa3O%2BEN7dtWTe3OOYvv5w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oj23bdqM-PdD2J7X49vXeNBxEWfnLNHbPp4Jex1ZNugOA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...