Re: [MW:31470] ASME-Section-2C-SFA 5.23 - Spec for Low Alloy electrodes and Fluxes for SAW-Two run classification

Dear Mr Sandeep Mehta, 

i think you are mistaken. Pls refer to SFA 5.23. There it is clearly stated two run. 
Also i dont think there are tubular electrodes for SAW.

Tubular are for FCAW in which the flux is stored in the core, thus requiring the electrode to be tubular. 

On Friday, 18 September 2020 at 10:09:57 UTC+5:30 vyo...@gmail.com wrote:
Hello,

T - means Tubular and not Two runs.

Regards
Sandeep Mehta 

On Sep 17, 2020, at 02:56, Ramin Kondori <ramink...@gmail.com> wrote:


Dear Zacharias,

This is an example of a Two-run test sample
<Two run test.jpg>


This is an example of an All-weld metal test sample
<All weld metal test.jpg>


And this is an example of a Multi-run test sample
<Multi-layer test sample .jpg>



Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Fri, Sep 11, 2020 at 10:14 AM Zacharias Rohith Joseph <rohithj...@gmail.com> wrote:
Hello Everyone, 

In SFA 5.23, in the electrode classification, there is a character "T", which is defined as a designator for two run electrodes. 

What does this signify and how is this different in operation from the normal SAW electrodes. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e7db420-2d21-455d-9199-c8b39f64ffccn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed017e9d-2799-487f-86a9-961eb5d6d473n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...