Re: [MW:31467] ASME-Section-2C-SFA 5.23 - Spec for Low Alloy electrodes and Fluxes for SAW-Two run classification

Hello,

T - means Tubular and not Two runs.

Regards
Sandeep Mehta 

On Sep 17, 2020, at 02:56, Ramin Kondori <raminkondori@gmail.com> wrote:


Dear Zacharias,

This is an example of a Two-run test sample
<Two run test.jpg>


This is an example of an All-weld metal test sample
<All weld metal test.jpg>


And this is an example of a Multi-run test sample
<Multi-layer test sample .jpg>



Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Fri, Sep 11, 2020 at 10:14 AM Zacharias Rohith Joseph <rohithjoseph18@gmail.com> wrote:
Hello Everyone, 

In SFA 5.23, in the electrode classification, there is a character "T", which is defined as a designator for two run electrodes. 

What does this signify and how is this different in operation from the normal SAW electrodes. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e7db420-2d21-455d-9199-c8b39f64ffccn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUjKspOuVfHvz2Z8bXm8MsvXQgSXsneR-_iURAS1akub_A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...