Thursday, September 17, 2020

Re: [MW:31463] brittle fracture CS 516 Gr.70N

Dear Ramon,

Could you share the test results (the lab roport)...?
Has the samples failed in weld metal or HAZ...?
Additionally, please provide us with other test results (tensile test, macro, etc.).

Details are very important here.

Regards 
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Mon, Sep 14, 2020 at 7:04 AM Customer Care <bricenori@hotmail.com> wrote:

Dear Fiends,

I have a question about how excessive heat input affects SAW type welding, in a steel SA 516 Gr. 70 N. That is, a material subjected to Charpy test at -45C, and gave brittle fracture with absorbed energy between 4 to 6 lb-ft.

The WPS / PQR clearly rated, but shop production welding gave these results on pressure vessels.

My certainties indicate that coarse-grained ferrite and widmanstatten ferrite could be formed during the cooling of the weld (highly brittle), and not the expected acicular ferrite, which is the appropriate structure for excellent ductile fracture results in this type of steel.

 

I open the forum,

 

Thanks for your attention.

 

Regards,

Ramon Briceno

Sent from Mail for Windows 10

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL0PR03MB4243D9B14CD62401925CA39FAA220%40BL0PR03MB4243.namprd03.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUidzGPHkE%3D%3D4sQKZerN2-q5TqXG-4xsdz5_OinMEo1zNA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...