Dear Mr. Nazeer & All,

Weldolet comes with a Reinforcement which increases Thickness and OD and can it be considered like a Pipe.

Any reference of Code Interpretation with respect to Weldolet for welder qualification.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 16 September, 2020, 01:38:55 pm GMT+7, Nazeer <naz.mhd@gmail.com> wrote:


Dear Mr.Murali,

Table QW-452.3 specifies the Outside Diameter of pipe, fitting, etc in Inch & mm units. Its not specifying the pipe size in NPS or DN.

Hence OD 73 mm & over qualified welder is qualified to weld 82mm OD .

For better understanding, refer the Table QW-452.3 in mm unit for 82mm OD

Thanks & Regards
Nazeer

On Wednesday, September 9, 2020 at 6:57:24 AM UTC+3 MK wrote:
Greetings,

I have a weldolet 2" NPS X OD 82 mm, I want to use the welder qualified for 2 7/8 (73 mm) & over.

Query initiated by client that as per ASME SEC IX Table QW 452.3 foot note (b) states that 2 7/8 in. (72mm) O.D. is the equivalent of NPS 2 1/2 (DN 65). In this case the welder client says welder is not qualified for 2 inch NPS.


since the welder qualification essential variable is OD inline with ASME SEC IX, kindly advice.

If any reference kindly share the same.

Thanks 
Murali


--
 
 
Thanks and Best Regards,
 
G.Murali krishnan
Mob : +966-501487307
Saudi Arabia

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/ed45ba87-1a14-47b2-8fbf-e5397b627719n%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...