Monday, September 21, 2020

[MW:31488] Clarification regarding Thickness range

Dear Experts,

Please need your response on my doubt.

PQR Details as below - ( For piping line classes ASME B31.3 and Sec.IX ).
Base metal Thickness - 30.96mm 
 Impact Tested with - @-29°C
PQR Based on a dual process GTAW+SMAW ( 4.0 mm+26.69 mm).
Material - ASTM A106 Gr.B

My Doubt as below - 
Shall I use the range in my WPS - 
Base metal Thickness - 25.4 mm to 36.96 mm.
dual process GTAW+SMAW  Range - 8.00mm to 28.96mm. 

OR
 Shall I follow QW-403.6 and for Impact test Shall  refer range - ASME B31.3 Table 323.3.1 (A-5) T/2  to T+6 mm.

Or
If I need this qualification - the above mentioned range in WPS is acceptable -  ( i.e - 25.4 mm  to 36.96 mm).

Please give me your response on my doubt with code reference. 

Thanks in advance.

Regards 
Kiran




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a167831-2c8c-41e6-9b4e-11878490c311n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...