[MW:31483] ASTM G28- Retest

Greetings all
In one of our project, G28 Method A for Inconel 625 pipes (B444) didnt met the accpetance criteria - (one sample didnt meet in the weight loss requirement) and other didnt  meet the 50X magnification requirement. 
The supplier is cross referring to MR0175 Part C and requesting for retesting. But  is MR0175 right document to cross refer? Any thoughts?

Regards
Nitin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cd8705e4-5718-4ace-b75c-8adc3dc95402n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...