Friday, September 11, 2020

[MW:31426] ASME-Section-2C-SFA 5.23 - Spec for Low Alloy electrodes and Fluxes for SAW-Two run classification

Hello Everyone, 

In SFA 5.23, in the electrode classification, there is a character "T", which is defined as a designator for two run electrodes. 

What does this signify and how is this different in operation from the normal SAW electrodes. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e7db420-2d21-455d-9199-c8b39f64ffccn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...