Monday, September 30, 2019

Re: [MW:30096] F‐No. 6.

F no may not be issues. Only weld metal A no may be issues. 

On Mon, 30 Sep 2019 10:54 am 'Raja kumarasamy' via Materials & Welding, <materials-welding@googlegroups.com> wrote:


Dear sirs,

kindly advise on the below query.....


 Deposited weld metal made using a bare rod not covered by an SFA Specification but which conforms to an analysis listed in Table QW-442 shall be considered to be classified as F‐No. 6.


 Regards
Raja 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/894699591.406112.1569676100044%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM7zwNWJdDhX-yvkhL2teKbC6Yu7mFD2%2BR%3DNRrt0Lt82w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...