On Mon, Aug 12, 2019 at 5:40 PM 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi!Pl clarify1)a)Does Dishend.have weld seam which ll undergo normalsing? After formingIf yes you wiil req qualified.WPS/pqr of normalise +pwht below Ac1 as per code for P1b)If no then you need not.have pqr of Normalising but only Pwht below Ac1 as per code for P12) in case of condition (a) you should have 2Pqr one with NR+pwht and second with pwht below Ac1In case of condition (b) only.one Pqr of pwht below Ac1 temp as per P1 matlRegardsHegde--
On Mon, 12 Aug 2019 at 15:44, chiluka venkatramulu<ramuluchiluka@gmail.com> wrote:Dear All,--Pl clarify the below.One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
- Dishends Normalising-2 cycle.
- PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?OROnly two normalising cycles are enough?Regards,Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdGvDLB4C3Y24JY-HL4JW2%3DC%2BUuXnw8sFhsPDo6-i0sKSg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1487532532.3710168.1565605847733%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKjKdNaJwEJQJo0cv78g3dxy1HaaRz8qxoLi5KW4uwFisNpV0A%40mail.gmail.com.
Comments