Dear Basem
If you have 14 joints in one tank you have take 7 spots in any 7 joints .
Regards
Sangramkeshari Routaray
Welding inspector
Sent from my iPhone
Dear, sangramWhat the meaning of radial joint ?Thanks for your cooperation--On Mon, Sep 9, 2019, 07:53 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:Dear Basem--Yes as per API-650 you need to be radiograph at least one spot on 50% of total joints.RegardsSangramkeshari RoutrayWelding inspectorSent from my iPhone--Dear allAre the but welding joint in annular plate of tank must be RT or not as per API 650?Thanks
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACct1WHdS23%2BJ-gP9DybDPqfOqqUKDssOugYqYAjrY%2B8zYrEgg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/890DE5AF-2731-4DD0-888E-3D0625358EFC%40yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACct1WF4-%2BVWE5By%2BpJGrdeT%3DL_GPqWZxEj1wPWQPV-ozFjdaQ%40mail.gmail.com.
Comments