Monday, September 9, 2019

Re: [MW:30040] Re: Change groove type in D1.1

Thank you very much.

I don't know why summary PQR of my company or summary PQR of other company has all joint design (single V, single B, double V, double B). If 1 PQR with 1 joint design can qualify for other joint  design, why they must cost money for them.
(sorry, my english is not good)

Thank Experts

Regards
Nguyễn Nhật Hoàng

Vào Th 2, 9 thg 9, 2019 vào lúc 10:54 Bien_ND / weldinginspections.net <bck055@gmail.com> đã viết:
On Thursday, September 5, 2019 at 10:15:44 AM UTC+7, Nhật Hoàng Bk wrote:
> Dear Experts,
>
>
> Could you please advise me for a question:
> I have a PQR qualifies single V, can I write WPS for single V, doubleV, single Bevel, double Bevel.
>
>
> Thank Experts

Reduce angle bevel are not allowed.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1deb3f5c-b994-4037-b596-fcb72c792fc0%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM8%3DVVF%2BH_4b2oP1CQx0w6reU1%2BsZ%3DCnqf%2BG%2BLeGTY5S0FSM7g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...