first to think wps is for weld .so your weld is facing only pwht so you have to quailfy wps by pwht only , normalizing of dish head to do separately.if dish head is welded than wps to qualify with normalize + pwht in isngle coupon as per sec 9
On Monday, 12 August 2019 15:44:19 UTC+5:30, chiluka venkatramulu wrote:
-- On Monday, 12 August 2019 15:44:19 UTC+5:30, chiluka venkatramulu wrote:
Dear All,Pl clarify the below.One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
- Dishends Normalising-2 cycle.
- PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?OROnly two normalising cycles are enough?Regards,Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2996f76d-c2b5-4ef0-a940-36c4576f5a46%40googlegroups.com.
Comments