On Saturday, August 31, 2019 at 1:53:08 AM UTC+7, Raghul wrote:
> Welder made two coupon
> 1. Coupon with 6 mm thickness on the 1/2" pipe made by gtaw process
> 2.coupon with 15 mm thickness on 2-7/8" pipe made by gtaw+smaw process.
>
> Is the welder qualify to weld on 1/2" pipe with gtaw+smaw process for qualified thickness?
>
> Please explain
which standard for qualification?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c5f79021-f4f6-4a6a-a575-8423d60f02fc%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment