Dear all,
Need to establish a WPS For a project with PWHT root(full penetration by SMAW)and Subsequent layers by (SAW).
My doubt is I have two seperate WPS for each procedure with PWHT separately.
Can I submit both WPS to client and use them as one procedure on job
1. Root- full penetration joint - SMAW
2. SUB sequent layers - SAW
NO Backgouging will be done.
Root and finish to be UT 100%.
REGARDS,
DATTU.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1fe7d9fd-d244-4aea-ae2d-8bcda3ae1316%40googlegroups.com.
Need to establish a WPS For a project with PWHT root(full penetration by SMAW)and Subsequent layers by (SAW).
My doubt is I have two seperate WPS for each procedure with PWHT separately.
Can I submit both WPS to client and use them as one procedure on job
1. Root- full penetration joint - SMAW
2. SUB sequent layers - SAW
NO Backgouging will be done.
Root and finish to be UT 100%.
REGARDS,
DATTU.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1fe7d9fd-d244-4aea-ae2d-8bcda3ae1316%40googlegroups.com.
Comments