Re: Re: [MW:28480] Re: Difference between the electrode E8018 B-8 & E8015 B-8

without leaving room for confusion and as mentioned earlier trailing mail CVN is not applicable in your case, go ahead without qualifications.

Regards,
Muneeb.M
 
Date: 2018-10-22 10:29
Subject: [MW:28470] Re: Welding Electrodes
E8016-B2 is having increased Cr. compare to E8016-B1.
Please elobrate more, what is the reason for change & any code compliance applicable.

According to ASME section IX,  QW 404.12 its a supplementary essential variable and require re-qualification if you have CVN requirements.
 
Thanks & regards
Sandeep Kumar



 
Date: 2018-10-18 16:14
Subject: Re: [MW:28435] Re: Difference between the electrode E8018 B-8 & E8015 B-8
Dear expert,

can we use welding electrodes E8016-B2 instead of E8016-B1?

Answer: change in classification is falling under supplementary essential variable and your case can be used as per QW-404.12, which does not clash with a to f. 

Can any body differentiate between the electrodes E8018 B-8 & E8015 B-8, and the difference of applicable areas.
Answer: 
A5.5                      A5.5M                    Type of Covering                                          Welding Positionsfor Classification(B)                Type of Current(C)
E8015-X              E5515-X            Low hydrogen sodium                                           F, V, OH, H                                                                 dcep
E8018-X              E5518-X          Low hydrogen potassium, iron powder(F)               F, V, OH, H                                                               ac or dcep

Regards,
M.Muneeb.



 
From: mathafiza
Date: 2018-10-17 04:08
Subject: [MW:28435] Re: Difference between the electrode E8018 B-8 & E8015 B-8
Dear expert,

can we use welding electrodes E8016-B2 instead of E8016-B1?

On Saturday, January 5, 2013 at 1:50:29 PM UTC+8, Biplab Pal wrote:
Dear Experts,

Can any body differentiate between the electrodes E8018 B-8 & E8015 B-8, and the difference of applicable areas.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...