Wednesday, October 31, 2018

Re: [MW:28533] SA335 Gr.P91(P-15E)

table 331 in b31.3 - pwht , 341 for ndt

regard
rajesh

On Wed, Oct 31, 2018 at 7:36 AM 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear experts ,
If some one have working experience with p91 material; please help regarding heating & cooling rate. Max hardness allows .
My construction code is Asme B31.3
Please specify the code details.

Sent from my iPhone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...