Sunday, October 28, 2018

Re: [MW:28510] RE: 28480] Welding of UNS31254

Thankyou sir for your valuable reply.
I am trying ESAB ERNiCrMo-3 for GTAW and ENiCrMo-3 for SMAW.

On Sat, 27 Oct 2018, 5:28 am PGoswami, <pgoswami@quickclic.net> wrote:
Hi,

Please see the attached document providing detailed  information on UNS 31254 steel, including welding. Recommended consumables are highlighted. Usually Inconel  625(ER-NiCrMo3) is the preferred grade for   this alloy. The other grades are recommended based on the design criteria.
You should check with reputed manufacturers, on the best recommendation.
I had dealt with Metrode  products in the past. However there're other good manufacturers also.

Thanks.

P.Goswami.P.Eng, IWE.
Welding & Metallurgical Specialist

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Darshan Revdiwala
Sent: October 22, 2018 12:43 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28480] Welding of UNS31254

Can anyone share practical experience for welding of UNS 31254 and consumables selection for Tig and SMAW process.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...