Monday, October 22, 2018

Re: [MW:28477] Weld overlay

It is preferable to use E Ni electrode as barrier layer. 
Regards.,
Prasad G. 

On Mon, 22 Oct 2018 13:52 P.K.Pal, <palpk07@gmail.com> wrote:
Dear experts,
Due to Fe content issue & to achieve undiluted chemistry of Monel 400, on CS materials, whether, it will be better to use ERCuNi weld as Barrier layer on CS materials and then to deposit the weld overlay with ERNiCu7. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...