Dear Pankaj,

Holiday test can be carried out on coated surfaces.

Regards,

R.Ravi,

9881598398.
--------------------------------------------
On Sun, 21/10/18, deva m <devmunch@gmail.com> wrote:

Subject: Re: [MW:28463] Holiday test
To: materials-welding@googlegroups.com
Date: Sunday, 21 October, 2018, 10:04 AM

Holiday test can be
performed on any coated surface only thing we should ensure
is pipe/plate material should be electrical
conductor..
There is no
effect on material due to spark occurred in holiday
test..
RegardsDhevendran.
M

On Sun, Oct
14, 2018, 12:08 PM Pankaj Kolhe <pankaj.kolhe15@gmail.com>
wrote:
Dear experts Can we perform hoilday test on
painted surface of SS316L spools.

pankaj



--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.





--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...