Sunday, October 21, 2018

Re: [MW:28462] Holiday test

What about sparking? So, better try Dye Pen.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Saturday, 20 October, 2018, 8:46:25 PM IST, Tomas gonzalez <tomason11@gmail.com> wrote:


Sorry, yes you can. Because SS os also electricty conductor.

In muy previous email I made typing mistake, thinking one thing and writing the opposite, sorry.

El sáb., 20 oct. 2018 12:31, rajesh kaswala <rajeshkasvala@gmail.com> escribió:
so what method check for homogeneity of paint on ss 316 spool

regard
rajesh

On Thu, Oct 18, 2018 at 2:49 PM Tomas gonzalez <tomason11@gmail.com> wrote:
No you can't, this test is performed on a nonconductive coating applied to an electrically conductive surface.

El dom., 14 oct. 2018 8:38, Pankaj Kolhe <pankaj.kolhe15@gmail.com> escribió:
Dear experts
 Can we perform hoilday test on painted surface of SS316L spools.


pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...