[MW:28498] Using API 5LX65 FLG instead of A350 LF2 during qualification of A333 GR 6 P1G1 to P1G2

Dear Expert,

Is it possible to replace LTCS Flange A350 LF2 by Flange API 5L X65 during qualification of A333 GR 6 Pipes to A350 LF2 Flange.

--