[MW:28470] Weld overlay

Dear experts,
Due to Fe content issue & to achieve undiluted chemistry of Monel 400, on CS materials, whether, it will be better to use ERCuNi weld as Barrier layer on CS materials and then to deposit the weld overlay with ERNiCu7. 

--