Monday, October 22, 2018

[MW:28463] RE: 28417] Holiday test

Yes you can like any other conductive surfaces.

 

 

With best regards,

Firoz Ahmed (Umar), PMP®, MICorr®

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pankaj Kolhe
Sent: Sunday, October 14, 2018 9:36 AM
To: materials-welding
Subject: [MW:28417] Holiday test

 

Dear experts

 Can we perform hoilday test on painted surface of SS316L spools.

 

 

pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...