Hi..
Good question.. I would like to add possible option say that we qualify a PQR joining the P11 with P91 with the B2 or B6 electrode and make full destructive test to evaluate the weld soundness and the weldability...
Once we have valid PQR and pass all the test consider that sufficiently enough be used at Site.
I know this not the right solution but maybe an option from the Contractor who like to take advantage..
Thanks
Ghafor
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Good question.. I would like to add possible option say that we qualify a PQR joining the P11 with P91 with the B2 or B6 electrode and make full destructive test to evaluate the weld soundness and the weldability...
Once we have valid PQR and pass all the test consider that sufficiently enough be used at Site.
I know this not the right solution but maybe an option from the Contractor who like to take advantage..
Thanks
Ghafor
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments