Re: [MW:26105] GMAW+SAW-Welder/Welding operator Certificates as per ISO9606-1 or ISO14732 or combination of Both STDS
9606-1 covers only manual and partially mechanized welding. If your SAW is mechanized as per definition of 14732 then you need to involve both standards
2017-02-19 7:37 GMT+02:00 Kannayeram Gnanapandithan <kgpandithan@gmail.com>:
--
A welder was qualified in combination of GMAW(Semiauto)+SAW(Mechanized) . Whether Certificate is to be made as per ISO9606-1 or ISO14732 OR combining both stds??THANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITYMobile no: +919940739349
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .CAJzm4eMrG%2B3QdsU_ wqdwvOuswkQd1g% 2BPe9uZsbXtAhO4b5o-WA%40mail. gmail.com
For more options, visit https://groups.google.com/d/optout .
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D_n-JGsJ_1WOhmxkn8%3DQR2bqHngm2-dh1Nx0HxMs%3DJdw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments