Re: [MW:26101] Re: Regarding 2% sensitivity in radiography film.

Even in case of double wall technique, when you want to calculate sensitivity you consider the single wall thickness

2017-02-16 16:03 GMT+02:00 Prasad Rode <purode333@gmail.com>:
Dear sir,

Mr, srinivasan sir, given calculation for double wall technique and 1" dia, but instead of that if it would be single wall or big dia., then that calculation will not work.

My understanding is that Mr, George sir given guideline to refer SE1025, and that section shows  that 2% sensitivity is related to X-YXX in that way.

I expain the concept which i understand it, in last button one mail, and so requesting also to George sir, pls clear that my understanding is proper or not.


Pls reply, if anyone has query.
I think, it is very important to clear the concept of sensitivity, specially 2% sensitivity, which is normalky given in every Radiography format.

I want to clear the concept, which can help others for future.

Regards
Prasad Rode

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8567de6f-a1dc-4da8-94eb-bf824c97c1cf%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AzH7PKeBtQh-CWuqsmiHmDw_CzUa%2Bi5zJaNkweXO8x%2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...