Dear Sir,
Your calculation is wrong and I think you are not understanding the concept of senstivity calculation and selection of IQI.

2% of sensitivity of 4.1 mm thk would be 0.082mm and the IQI wire diameter of 0.082mm shall be visible in the film. 
So you have select as per ASME Sec V Table 233.2 ,  set B to be used.



Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +9184695933

Sent from RediffmailNG on Android




From: Rajendra Jadhav <raj04aug@gmail.com>
Sent: Thu, 16 Feb 2017 17:18:05 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26085] Regarding 2% sensitivity in radiography film.

Refer UW-51

On Tuesday, January 10, 2017 at 11:43:00 AM UTC+5:30, Prasad Rode wrote:
Dear sir,

I have 1" s.s. pipe having thkness of 4.1mm. We have used x ray quality with D4 size film. We have shown the client, required IQI as per sec V.

But client wants 2% sensitivity as per specification.

Sensitivity= min thk of visible wire/ thk of base metal*100

In our case, sensitivity= 0.20/4.1*100.      
So, it will come as 4.84 % .

So, how we will get 2% sensitivity.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/6f7a9e22-efdb-4513-a455-a33fb7e816ba@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1487247474.S.49084.autosave.drafts.1487248172.24849%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...