Re: [MW:26070] Lateral TEE joint RT

RT can not be performed with accuracy, can do UT in substitute of RT

On Thu, Feb 2, 2017 at 6:45 AM, Dinesh Patil <dinn.patil@gmail.com> wrote:
Any one can tell me ,can we do the Radiography test in lateral tee joint?.

--

Dinesh S Patil 

Welding and NDT Coordinator

 

 SEPCO Electric Power Construction Corporation

Saudi Aramco Master Gas System Expansion-Phase – II

Tel:- 00971 (04) 208 7249, Mobile: 00971- 527743152

Office Address – Conrad Tower,

P.O BOX: 242473, Sheikh Zayed Road, Dubai, UAE

Email: dinesh@sepco.net.cn , Website:http:// www.sepco.net.cn

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPaX8ZJBK_%3DjT3T7i9%2BC%3DvyXkMpNi-YYhV1M%2B4pj-G725yLkOA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B8iniEivfbECVS%3D8GzosYq%3Da-NOaFTsCCYiJbyUS4xi7Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...