Skip to main content

[MW:26119] Re: GOST 1050-88 CT 3

Please tell me Equivalent grade materials for CT-3 
steel. 

On Monday, January 12, 2009 at 7:46:48 AM UTC+5:30, aior wrote:
Hi,
I worked in Russia and hope to share some info with you. The problem
is that Russian standards and specifications are different from ASTM:
There are different GOSTs for different products for the same CT-3
steel.

Steel CT-3 is no longer listed in GOST 1050-88, it is now listed in
GOST 14959-79 which is a product specification for Carbon and Alloyed
Spring Rolled Steel.

In addition, the same steel is listed in various product
specifications:
GOST 535-88 for round bars and shapes.
GOST 14637-89 for plates and sheets.
GOST 8479-70  for forgings.

Typical chemical composition for CT 3 (killed) is: C (0.14-0.22), Si
(0.15-0.30), Mn (0.40-0.65)
Mechanical properties: YS 225-245 MPa min, TS 370-480 MPa min, A
22-26% min (depending on the product thickness). So, it is very close
to A-36.

Hope, it is helpful
aior
Oregon, USA


On Dec 16 2008, 5:54 pm, bagesh....@gmail.com wrote:
> GOST 1050-88 CT-3: Carbon structural quality steel gauged bars with
> special surface finish. General specifications [Replaced By: GOST
> 14959]: Carbonaceous and Alloyed Spring Rolled Steel Specifications
> Incorporates Amendment 1: 11/1982, Amendment 2: 12/1985, Amendment 3:
> 12/1986, Amendment 4: 06/1987, Amendment 5: 01/1989, and Amendment 6:
> 02/1993 [Replaced: GOST 1050] The said standard has been replaced with
> GOST 14959: in which the Grade of Steel you desired is CT3(Russian):
> ST3(English) steels, general purpose steel for Structural steel usage,
> It comes in Various profiles known as Russian steel Profiles, the
> chemical composition of this material is almost same except that of
> Carbon content which is less than that of A36, and it can be used up
> to -70 deg C with impact testing, but before using I would suggest you
> to confirm its Yield strength and tensile strength by comparing the
> percentage elongation.
>
> KUMAR BAGESH
>
> On Dec 16, 6:07 pm, Kim <shihyue...@yahoo.com> wrote:
>
> > What is GOST 1050-88 CT 3? Is it equivalent to ASTM A36?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bf769bf3-cad7-46e2-b4ab-ff8bfcea2766%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...