Re: [MW:25457] RE: 25392] PWHT

It is controlled by the crystalline structure and more specifically:
  1. by the diffusion of atomic hydrogen
  2. by the capability to sustain the pressure of molecular hydrogen by plastic transformation
The increase of hardness is an indication of low ductility and thus less possibility of plastic transformation of the grains

2016-09-26 19:25 GMT+03:00 'Ahmed Eissa' via Materials & Welding <materials-welding@googlegroups.com>:

Regarding the belowmentioned
I need to confirm that HIC is not controlled by hardness control but by steel chemistry 

All shall be reminded that wet sour service induce 

Sulfide stress cracking
Hydrogen induced cracking 
Stress oriented hydrogen induced cracking 
Hydrogen blistering 

Nace MR 0175 or nace MR 0103 only control ssc, please read these code introduction /preface 

Ahmed eissa 
Materials and Corrosion Engineer 




On Thu, 15 Sep, 2016 at 5:38 am, pgoswami

Hello, ZHY370137,

 

I'm not sure why you're asking this question is general forum, when your contract is bound by your clients' specifications and project requirements. Aramco has very comprehensive specifications for almost everything. If Aramco SAES-W-012 is applicable for your project you need to what's needed as per this spec.

 

What's  the design code, of the pipeline B-31.4 or 31.8? And what're the Aramco specifications applicable?

 

Usually for sour service hardness control is "mandatory" to mitigate the HIC. One of the effective ways to ensure hardness control is PWHT, unless vendor is able to prove otherwise.

 

Appreciate your response.

 

Thanks.

 

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of zhy370137@gmail.com
Sent: Wednesday, September 14, 2016 10:59 AM
To: Materials & Welding
Subject: [MW:25392] PWHT

 

Dear sir

good day 

pls hlep us confirm whether we need apply PWHT for every girth weld according to your experience.

pipe API 5 L X60 HIC resistant pipe

welding method: CRC automatic

pipeline diameter and thickness:20inch 0.4inch(10MM)

mediumsour condensate 

pressure:960psi

pipeline distance164km between two gas plant in saudi safaniya plant to berris gas plant)

clientsaudi aramco

 

CNPC daqing saudi 

QAQC

 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f49f77aa-d202-4cc2-91c7-b5f1f828afcd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/866914810.4904114.1474907104598%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D8h6p9fJxADQA9iUi716b96mqALy8yzX6a602m7MQHWg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...