It is the lower transformation Temperature 725degC

2016-09-25 19:04 GMT+03:00 Ankit Gandhi <asgandhi.90@gmail.com>:
Dear as per ASME viii div.1 you have done simulation which is represent material property after pwht so you can rise temperature up to that simulation cycle.

Regards,
Ankit

On Friday, 10 February 2012 00:48:11 UTC+5:30, Tariq Hussain wrote:

Dear Friends,

 

minimum PWHT Soaking temperature is given in ASME Sec VIII Div. 1 UCS-56, My question is What is maximum temperature that we can use for PWHT with reference to some applicable standards or metallurgical point of view point?

 

OR

 

Can we do PWHT for P.No.1 Gr.1 & 2 (e.g SA 516 Gr. 60 & 70) maximum up to lower critical temperature i.e. 723 Degree Centigrade?

 

Thanks in Advance for your valuable share.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/93543276-32bd-405c-9a09-5ec4150e8c7f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Ayw6Uo7ddSvqeh8f8EkMokS-i6xfVjO778u%2BUv4jm7NQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...