Re: [MW:25414] UT/RT

There is no such code or standard, which compel you to perform  after 24/48 hours of welding.
However, it is recommeded to perform it  early inorder,  to know the soundness &  quality of the weld as well as performance of welder .
Thanks

On 14 September 2016 at 21:56, Sundar Kumar <sunkumarshine@gmail.com> wrote:
Dear Experts,

  Is there any code reference that we should do  UT/RT only after 24/48 hours of welding . We are following construction code 31.3. Material carbon steel .

Thanks&Regards,
Sundar 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a90c58bb-0889-4883-acd2-a4a896e68802%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMXKe_p8gVSz_%2B0BfKPR%3DbGLJ4tR3rJHvs0t0M0X2ysyAcP0bw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...