Re: [MW:25396] RE: 25392] PWHT

Dear pgoswami:

Thank you for your reply!

PIPELINE design code is B-31.4/31.8 , Aramco specifications is SAES-W-012 and design office  is SNC- lavalin
the pipeline is LSPB contract and  in bidding phase, but design discription about PHWT just  is acoording to standard and spc  .
But we just find  hardness control for sour services in the above document (girth weld and HAZ hardness is more than 250 HV10)
According to my experiences, girth weld and HAZ hardness of X60 mterial is lower than 250 HV10 without PWHT.(EVEN like this ,in other country iraq or iran ,we need apply PWHT for girth weld because feed design requirment)
So pls help us confirm whether girth weld and HAZ Apply PWHT or just control hardness,because it is the first bid  in the saudi aramco.

thank you 

CNPC daqing saudi 

QAQC

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of zhy370137@gmail.com
Sent: Wednesday, September 14, 2016 10:59 AM
To: Materials & Welding
Subject: [MW:25392] PWHT

 

Dear sir

good day 

pls hlep us confirm whether we need apply PWHT for every girth weld according to your experience.

pipe API 5 L X60 HIC resistant pipe

welding method: CRC automatic

pipeline diameter and thickness:20inch 0.4inch(10MM)

mediumsour condensate 

pressure:960psi

pipeline distance164km between two gas plant in saudi safaniya plant to berris gas plant)

clientsaudi aramco

 

CNPC daqing saudi 

QAQC

 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f49f77aa-d202-4cc2-91c7-b5f1f828afcd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAKk2HhFTkdJFmiQx6rgJZZIBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPaWuoGuH0G21Se7rckaoHfPnV3Aj9M7-Hfk%2BDoaAFUQMNQe7Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...