Tuesday, September 13, 2016

Re: [MW:25381] WPS requirements according to PQR

I wonder that Impact test is not required, unless the thickness is lower that 13 mm. SA-333 belongs to the curve A of UCS-66M.
if impact test is not required, then you can use the available PQR provided that all other essential variables are within range

2016-09-10 16:34 GMT+03:00 Himanshu Panchal <mec4him@gmail.com>:
Dear All,

I want to prepare a WPS for SECVIII Div-1,Material-SA333, MDMT: -46C,Thickness 24 mm.

As per vessel drawing there is no impact test and PWHT requirement.

I have one PQR without impact test.

Can i prepare the WPS based on that PQR who is with out impact test?

MDMT of vessel is -46C.



Thanks & Regards,

Himanshu panchal

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHjqA0P6GGCHuozpPeM7P0f5KuaQJhh0CiS1MHYdkrFNqp0Kw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Azmo7R7B2_btBTgrY8-9Fq6j9%2BQ_VPPSkm488edUALHA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...