Dear sir / experts, 

I need help for welding a M.S. Pipe  with Mechanized FCAW Process for root pass to get good penetration for X-ray ( without backing strip & back gouging ) Wire, E71T-1. Dia, 1.2 mm.  Shielding  Gas,  100 % CO2.  Pipe  Dia  200mm. Wall Thickness 08.00mm. Welding  Position 1GR.

Please give me some guidelines  for above welding operation . Like,  voltage, Amps, and wire speed, travel speed, stick out,  torch angle, gas flow rate for root run  & other subsequent  run.

Few Engineers say that FCAW  are  not be recommended for open root run. They advised for  root  run  weld with GMAW process & subsequent run  by FCAW process. And I found in  ESAB Welder Guide Book . Page No. 16.  they are also  not recommended  root run  by FCAW.  on Pipe  &  Plate both.

My queries are as follows :

1.     Is it possible to weld a root run for X quality penetration  with  FCAW Process?

2.    There is any restriction for root  run welding  with FCAW   by any Welding Codes  like ASME Sec. IX, AWS D1.1. or  ISO 15614. ?

Thanks & Regards.

G. K. Banerjee.

Welder  Trainer.

NAGPUR. ( India )

M-09764555112. 09423632112.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGhQL0%3DnDGJ5RRxMhwwPd1ksrOp8oomsL_w%3DQ%2Bi06z-KsdLdmA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...