Dear Experts,
I would like to have a discussion regarding "pre- heating & its
mainatances" for aPressure vessel weldings ( ASME SEC. VIII DIV.1,
shell thickness -55mm & dish end -65mm, material SA 516 Gr.70, vessel
length -18mtr & ID-3mtr). WPS is calling for pre-heating of 100 deg.
C.(maintainace required for joints above 25 mm thickness) project
location - GCC.
Welding processes - LS & CS - SAW. Nozzles- SMAW.. since due to the
high ambient temp. of around 35-40 deg. & due to practical
difficulties, the welders could only maintain pre-heating while they
starting welding & not during the welding ( specially on the other
side of joints). the client insisting for continuous heating during
welding.
I want to request for the opinions from members how far pre-heat is
crucial in GCC environment especially in CS materials.
Thanks in advance,
Kumar
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp8uN-yxCiWCQOnvgzLTz7OLjjK%2By1p-ZnKH20Fn30oCUQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
I would like to have a discussion regarding "pre- heating & its
mainatances" for aPressure vessel weldings ( ASME SEC. VIII DIV.1,
shell thickness -55mm & dish end -65mm, material SA 516 Gr.70, vessel
length -18mtr & ID-3mtr). WPS is calling for pre-heating of 100 deg.
C.(maintainace required for joints above 25 mm thickness) project
location - GCC.
Welding processes - LS & CS - SAW. Nozzles- SMAW.. since due to the
high ambient temp. of around 35-40 deg. & due to practical
difficulties, the welders could only maintain pre-heating while they
starting welding & not during the welding ( specially on the other
side of joints). the client insisting for continuous heating during
welding.
I want to request for the opinions from members how far pre-heat is
crucial in GCC environment especially in CS materials.
Thanks in advance,
Kumar
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp8uN-yxCiWCQOnvgzLTz7OLjjK%2By1p-ZnKH20Fn30oCUQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments