Thursday, September 15, 2016

[MW:25398] RE: 25392] Re: Requirements Of PWHT for the Cross Country Pipe Lines - Reg

The point is that you qualified the procedure with PWHT and so you are saying by that 'I intend to post weld heat treat the welds'. The solution is straightforward: requalify the procedure without PWHT, and see if that passes the requirements of the client specifications and the applicable pipeline codes.

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of zhy370137@gmail.com
Sent: 14 September 2016 16:03
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25392] Re: Requirements Of PWHT for the Cross Country Pipe Lines - Reg

 



201535日星期四 UTC+8下午6:36:41Amul Raj写道:

Dear Experts,

 

We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)

 

Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required 

 

Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT

 

What is the remdy for this & hat should we do 

 

Kindly drop your advise 

 

 

Thanks & Warm Regards,

 

Amul Raj T

 

QA/QC Welding 

 

Samsung Engg, KSA  

 

 

 

 

 

 

 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca086d47-ec6f-449f-8b79-7ba2446bbd11%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...