[MW:25396] Re: Using of ER70S-6 in place of ER70S-2

Please guide- If we add Ti in ER70S-6 in range of 0.011%, what will be the effect during CO2 welding?

regards,

Sanjeev

On Thursday, 10 January 2013 12:13:36 UTC+5:30, Ranendra Chakraborty wrote:
Dear Expert,
Please guide whether ER70S-6 can be used in place of ER70S-2. Please give code reference.
 
Regards,
Ranendra

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/07c21334-a631-40b0-b66e-65075cde9914%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...