在 2015年3月5日星期四 UTC+8下午6:36:41,Amul Raj写道:
Dear Experts,

We have done PQR with PWHT for the Material APL 5L Grade X60, and the coupon Size is 40 Inch & the Thickness is 38 mm with the Construction code application of API 1104 (Cross Country Pipe Line)

Based on the results we prepared WPS Also, But, As per API 1104 for 38.00 mm THK PWHT is not required 

Now The Aramco PID instructed to follow the WPS to do all the Joints PWHT

What is the remdy for this & hat should we do 

Kindly drop your advise 


Thanks & Warm Regards,

Amul Raj T

QA/QC Welding 

Samsung Engg, KSA  



 




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca086d47-ec6f-449f-8b79-7ba2446bbd11%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...